[Prev][Next][Index][Thread]

Re: Searching for Electode Material



The resistivity of zinc is about 2.5 times that of copper. melting point is
419.58deg C (copper 1084.5). Zinc actually oxidises in air at a far lower
temperature than this. Brass bolts and studding should be available from
many engineering suppliers, also try a boatyard or chandlers.
Steve
----- Original Message -----
From: Tesla List <tesla@pupman.com>
To: <tesla@pupman.com>
Sent: Friday, May 05, 2000 2:28 PM
Subject: Searching for Electode Material


> Original Poster: "Ryan Ries" <spud@wf.net>
>
> Hello, I'm looking for some better conductor for my air-blast gap than
> what I'm currently using.  I have 1/4" steel bolts for electrodes right
> now, and I realize that steel is not good, but I can't find any copper or
> brass or aluminum bolts.  (Isn't brass just copper with a sodium hydroxide
> shell?)  Also, does anyone have any info on the conductivity/heat
> dissipation of zinc?
>
> Thanks,
>        Ryan Ries
>                    http://spud.pureinsanity.net
>
>
>